MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Enriched 11 Boric Acid
Categories: Ceramic

Material Notes: Ceradyne, Inc., a 3M company, specializes in isotopic boron products for specific applications. Our manufacturing systems give us the flexibility to customize isotopic composition to meet customer requirements. 3M™ Enriched Boric Acid is one of the basics of our product line, and is a precursor for most of our other boron containing chemicals. Enriched in either isotope to very high levels, our boric acid exceeds accepted standards of the nuclear industry throughout the world. In chemical reactions, our enriched products behave the same as their natural counterparts. In a thermal neutron environment, Boron isotopes have opposing neutron capture cross sections. Whereas 10Boron is an extremely good neutron absorber, 11Boron is considered to be neutron transparent.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/cc
Molecular Weight 62.021 g/mol62.021 g/mol@ 99%
Vapor Pressure 0.0200 bar
@Temperature 180 °C
15.0 torr
@Temperature 356 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Formation -1096.87 kJ/mol-1096.87 kJ/mol
Decomposition Temperature 185 °C365 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B >= 99.95 %>= 99.95 %
 
Descriptive Properties
AppearanceWhite Crystals
Impurities<0.1 ppmPhosphates
 <0.12 ppmSulfates
 <0.26 ppmChlorine
 <0.3 ppmFluorine
 <0.5 ppmArsenic
 <1 ppmCalcium
 <1 ppmHeavy Metals (as Pb)
 <10 ppmWater Insolubles
 <2 ppmIron
 <3 ppmSodium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM40031 / 194922

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.