MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M 7735FL Acrylate Overlaminating Film
Categories: Polymer; Adhesive; Film

Material Notes: 3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers excellent clarity and provides at least five years of outdoor life, when used with 3M™ Polyester Label Stocks, as explained below

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.3 microns0.800 milAdhesive
 38.1 microns1.50 milLiner
 76.2 microns3.00 milFacestock
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.20817 kN/m1.1875 pliPolypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.20817 kN/m1.1875 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.27391 kN/m1.5625 pliStainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 79.0 °C174 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -12.0 °C>= 10.4 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type#400 Acrylic
LinerClear Polyester Liner

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33455 / 168202

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.