MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RSP Technology RSA-426 F/O Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached. As a result very fine nanostructured alloys with new functionalities are being developed and produced. A variety of shapes and sizes are available.

Information provided by RSP Technology BV

Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.59 g/cc0.0936 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6565
Tensile Strength, Ultimate 160 MPa23200 psi
Tensile Strength, Yield 90.0 MPa13100 psi
Elongation at Break 8 %8 %
Tensile Modulus 90.0 GPa13100 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C9.11 µin/in-°F
Thermal Conductivity 160 W/m-K1110 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 74 %74 %
Silicon, Si 26 %26 %
 
Descriptive Properties
Specific Stiffness35 GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NRSP46m / 320675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.