MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenciled or applied with an automated high speed dot dispenser.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/ccCured
Viscosity 2500 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79
Adhesive Bond Strength 1500 psiLap shear, alum to alum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00040 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°CBelow Tg
 120 µm/m-°CAbove Tg
Thermal Conductivity 2.00 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 175 °C
 1.50 hour
@Temperature 80.0 °C
 5.00 min
@Temperature 150 °C
 12.0 hour
@Temperature 50.0 °C
 15.0 min
@Temperature 120 °C
Pot Life 4320 - 5760 min(3-4 days)
 
Descriptive Properties
Color Silver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 23 Vinyl Hybrid Prepreg
Solvay XMTR50 (EF7313) Epoxy Resin System
Master Bond EP17HT-3 One component, snap-curing epoxy system
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Henkel Loctite® 3563 Epoxy Snap Cure Underfill

PTRAC196 / 71124

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.