MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grinding and master-batches.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.918 g/ccISO 1183
Linear Mold Shrinkage 0.020 - 0.040 cm/cm
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50after 15 sec; ISO 868
Tensile Strength at Break 7.00 MPaISO 527-2
Tensile Strength, Yield 8.00 MPaISO 527-2
Elongation at Break 120 %ISO 527-2
Modulus of Elasticity 0.150 GPaISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °CISO 11357
Vicat Softening Point 84.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 220 °C
Mold Temperature 30.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese 190 LDPE polymer for adhesives, automotive and compounds
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade
LyondellBasell Lupolen 1800U Polyethylene
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding

PTOTAL712 / 130437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.