MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman Diamond NPP25-0715CF20 20% Conductive Filler Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Impact Copolymer Polypropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792
Filler Content 20 %ASTM D5630
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.0 MPachs 2.0 in/min; ASTM D638
Elongation at Yield 100 %chs 2.0 in/min; ASTM D638
Flexural Modulus 2459 MPachs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 801 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® 25 CF/20 H Conductive Polypropylene
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Omni Plastics OmniPro™ HPP CCF20 Homopolymer Polypropylene, 20% Calcium carbonate filled
Celanese CoolPoly® E1201 Thermally Conductive Polypropylene
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene

PDIAM423 / 126514

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.