MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JIS SKS94 Oil-hardening Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: General purpose non-deforming low alloy for applications requiring extreme dimensional accuracy. Good abrasion resistance and toughness.

Key Words: JIS G4404(83) SKS94, SKS 94, SKS-94; Comparable to SKS21, SKS93, SKS95, AISI O1 Tool Steel, UNS T31501
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 212Hot Rolled Bar/Forging
Modulus of Elasticity 214 GPa(AISI O1)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.8 µm/m-°C
@Temperature 38.0 - 260 °C
(AISI O1)
 14.0 µm/m-°C
@Temperature 38.0 - 540 °C
(AISI O1)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 260 °CTempering Temperature (AISI O1)
 790 - 815 °CHardening Temperature (AISI O1)
Annealing Temperature 760 - 790 °C(AISI O1)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.90 - 1.0 %
Chromium, Cr 0.20 - 0.60 %
Copper, Cu <= 0.25 %
Iron, Fe 96 - 98.1 %As Balance
Manganese, Mn 0.80 - 1.1 %
Nickel, Ni <= 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
JIS SKS3 Oil-hardening Cold Work Tool Steel
JIS SKS93 Oil-hardening Cold Work Tool Steel
Crucible Steel KETOS® Tool Steel, AISI O1
Bohler-Uddeholm O1 Cold Work Tool Steel
JIS SKS21 Oil-hardening Cold Work Tool Steel

MSTZJSKS94 / 231087

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.