MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeoGraf GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
Categories: Carbon; Graphite

Material Notes: GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC can be used in a number of automotive or internal combustion applications. Additionally, GTC's ability to conform to less-than-ideally-finished surfaces is a benefit in aftermarket gasket applications. GTC is used in high-temperature sealing applications where binder-based materials fail. It is often combined with inserts to make head gaskets, exhaust manifold gaskets, EGR assemblies and filler material for heat shields. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 70.0 lb/ft³Standard
Moisture Absorption at Equilibrium 0.10 %
Thickness 380 micronsStandard
 510 micronsStandard
 640 micronsStandard
 760 micronsStandard
 890 micronsStandard
Ash 3.0 %
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Cl (Chloride) <= 10 ppmLeachable
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 650 psi
Compression Set 87 %
@Pressure 34.5 MPa
after 5000 psi load
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °C
Minimum Service Temperature, Air -240 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 97 %
 
Descriptive Properties
Compressibility (%)43at 5000 psi load

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
NeoGraf GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite

CGRAF926 / 107330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.