MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive
Categories: Polymer; Film

Material Notes: 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bubble-free installations and Removable without heat or chemicals

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 76.2 - 102 microns3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 17.2 MPa>= 2490 psi
Peel Strength 0.105 kN/m0.600 pliAdhesion to Glass
 0.298 kN/m1.70 pliAdhesion to Fruehauf pre-painted panels
 0.666 kN/m3.80 pliAdhesion to ABS
 
Processing PropertiesMetricEnglishComments
Processing Temperature 2.00 - 38.0 °C35.6 - 100 °FApplication Temp; Flat surfaces with and without rivets
 15.0 - 38.0 °C59.0 - 100 °FApplication Temp; Cured surfaces

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34798 / 169545

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.