Hydrophilic aliphatic polyisocyanate based on hexamethylene diisocyanate (HDI). As a hardener for aqueous two component polyurethane systems. Properties / Applications: Bayhydur® XP 2700 is a crosslinker for aqueous coatings. It was developed specially for trade applications where the ease of mixing the hardener by manual stirring is a key requirement. Information provided by Covestro |