MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel

ALVAR 14 is characterized by:

  • Good toughness
  • Good resistance to high thermal stresses
  • Good stability in hardening
  • Good through-hardening properties

Applications:

    Alvar 14 is ideally suited for hot working tools such as:
  • Support parts for extrusion tooling, e.g. backers, bolsters
  • Hot forging tools
  • Die for tin, lead and zinc alloys
  • Tools for hot shearing

Key Words: W.Nr. 1.2714; NiCrMoV7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³hardness of 40 HRC
 0.277 lb/in³
@Temperature 399 °C
hardness of 40 HRC
 0.279 lb/in³
@Temperature 199 °C
hardness of 40 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 250Soft annealed
 330 - 400Hardened and tempered (36-43 HRC, 1100-1350 Nmm2)
Modulus of Elasticity 31200 ksi(hardness of 40 HRC)
 26800 ksi
@Temperature 399 °C
hardness of 40 HRC
 29300 ksi
@Temperature 199 °C
hardness of 40 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.30 µin/in-°F
@Temperature 20.0 - 199 °C
hardness of 40 HRC
 7.70 µin/in-°F
@Temperature 3.33 - 399 °C
hardness of 40 HRC
Thermal Conductivity 36.0 W/m-K
@Temperature 20.0 °C
hardness of 40 HRC
 36.5 W/m-K
@Temperature 199 °C
hardness of 40 HRC
 36.8 W/m-K
@Temperature 399 °C
hardness of 40 HRC
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.55 %
Chromium, Cr 1.1 %
Iron, Fe 95.05 %As Balance
Manganese, Mn 0.70 %
Molybdenum, Mo 0.50 %
Nickel, Ni 1.7 %
Silicon, Si 0.30 %
Vanadium, V 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe LSS™ 2714T Hot Work Tool Steel (DIN 1.2714 mod)
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
AISI Type L6 Low Alloy Tool Steel (UNS T61206)
Armacell Monarch® F-05031 (Black) Neoprene, EPDM, SBR Blend Foam

NBUCOR06 / 15475

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.