System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NCMT NanoPAC™ N12 High Performance Polypropylene Nanocomposite
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
Characteristics:
Less shrinkage
Solved distortion problem
Good balance in impact and stiffness
High gloss
Reduce production cycle
Applications:
Household Industry
Toys Industry
Information provided by Nano Composite Materials Technology Limited
Key Words:
N Series
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.960
g/cc
0.0347
lb/in³
NCMT Method
Melt Flow
14
g/10 min
@Load 2.16 kg,
Temperature 230 °C
14
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
25.0
MPa
3630
psi
ASTM D638
Elongation at Break
>= 500 %
>= 500 %
ASTM D638
Tensile Modulus
1.60
GPa
232
ksi
ASTM D638
Izod Impact, Notched
1.25
J/cm
2.34
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
100
°C
212
°F
Deflection Temp.; ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Mearthane Durethane™ F DF-620A Closed Cell Foam Polyurethane
Mearthane Durethane™ F DF-225A Closed Cell Foam Polyurethane
316 Stainless Steel, annealed wire, 1.6 mm diam.
316 Stainless Steel, annealed sheet
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
PNCMT01 / 54726
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.