MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Ultrathene® UE635000 Ethylene Vinyl Acetate Copolymer, Extrusion Coating Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: ULTRATHENE UE635000 is an ethylene vinyl acetate copolymer recommended for extrusion coatings on cellophane, polypropylene and polyester. UE635000 is also used in special coextruded substrate coating applications, yielding improved heat stability for snack food packaging.

Regulatory Status: UE635000 is sanctioned by Food and Drug Administration regulation Federal 21 CFR 177.1350 and 21 CFR 175.105. These regulations (respectively) allow for the use of this material as articles or components of articles which are "...intended for use in producing, manufacturing, packing, processing, preparing, treating, packaging, transporting or holding food..." and as an adhesive which "...may be safely used as components of articles intended for use in packaging, transporting or holding food." Specific limitations or conditions of use may apply.

Processing Techniques: The maximum recommended melt temperature for UE635000 is 450°F.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D1505
Vinyl Acetate Content 9.0 %
Melt Flow 10 g/10 minASTM D1238
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 73.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 450 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
LyondellBasell Ultrathene® UE624000 Ethyl Vinyl Acetate Copolymer
Celanese Ateva® 2020 EVA polymer for coating lamination
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
Dow Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating

PEQU0810 / 104166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.