Hostacom TRS 217N is an unfilled PP copolymer, with excellent impact/stiffness balance, good flowability, very good scratch resistance and outstanding blooming resistance at elevated temperatures. This grade is delivered in customer customized colors, this Data Sheet reports general properties, some of them may be slightly altered upon color selected Avoid prolonged storage in open sunlight.Information provided by LyondellBasell. |