MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
A. Schulman tetra-DUR F 4001 Bulk Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: UL-Licensed, Abrasion resistance, free of fiber glass.

Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stability, color retention, chemical stability, zero shrink/class-A-surface, and uniform color.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 - 1.70 g/ccISO 1138
Linear Mold Shrinkage 0.0030 - 0.0050 in/inprocessing; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30.0 MPaISO 527
Flexural Strength 55.0 - 80.0 MPaISO 178
Flexural Modulus 5.00 - 8.00 GPaISO 178
Compressive Strength 130 - 140 MPaISO 604
Charpy Impact Unnotched 5.00 - 10.0 kJ/m²ISO 179
Charpy Impact, Notched 3.00 - 8.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Constant 4.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
@Thickness 1.00 mm
IEC 60243
Dielectric Loss Index <= 0.040
@Frequency 100 Hz
IEC 60250
Arc Resistance 180 secASTM D495-61
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CVDE 0304T1
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75
Flammability, UL94 V-0
@Thickness 19.0 mm
Shrinkage <= 0.10 %post molding; ISO 2577
 
Descriptive Properties
Water Absorption>80 mg/1dISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman tetra-DUR F 4308 Bulk Molding Compound
A. Schulman tetra-DUR F 4209 Bulk Molding Compound
A. Schulman tetra-DUR F 4206 Bulk Molding Compound
A. Schulman tetra-DUR F 4401 Bulk Molding Compound
A. Schulman tetra-DUR N 4203 Bulk Molding Compound

PBMC907 / 123371

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.