MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Random copolymer film grade

Color - Low catalyst residuals in FINA 6573XHC result in improved color stability.

Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and impact resistance over conventional homopolymer films.

Slip/Antiblock - FINA 6573XHC is formulated with no slip and high antiblock for specialized film handling.

FDA - FINA 6573XHC complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 6573XHC is recommended for use in manufacture of packaging films that require improved optical and impact properties.

Processing - FINA 6573XHC resin processes with typical melt temperatures of 450-525°F (232-274°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Water Vapor Transmission 11.0 g/m²/day
@Temperature 37.8 °C
90% RH; thickness not specified; ASTM E96
Melt Flow 8.0 g/10 minConditions not specified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %Non-oriented film; ASTM D882
Secant Modulus 0.690 GPa1% Secant Modulus; Non-oriented Film; ASTM D882
Dart Drop 1.40 g/micronF50; ASTM D 1709
Film Tensile Strength at Break, MD 48.3 MPaNon-oriented film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 148 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %Non-oriented film; ASTM D1003
Gloss 75 %45°; Non-oriented film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 232 - 274 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPR 8573 Polypropylene, Film Extrusion Grade
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break
Total PPR 8650 Polypropylene, Random Copolymer
Total PPC 3020 GN3 Polypropylene, Random Copolymer
Total 6571BB Polypropylene, Cast Extrusion Grade

PFIN81 / 38411

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.