MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: Properties:
  • Excellent mechanical properties
  • High thermal-chemical friction resistance
  • Good electrical properties
  • Good rate of melt flow index relative to the quantity of glass fiber
  • Balanced electrical and mechanical properties for flame retardant types
  • High toughness
  • Color and stability in high temperatures
Application:
  • Polyethylene with high density is widely and safely used for the manufacture of big containers for the transportation of kerosene and chemicals
  • Car oil and fluid by dye blow moulding processing
  • In the manufacture of shampoo and cosmetic bottles
  • In the manufacture of pipes and carrier cases

Key Words: PET
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.456 g/ccISO 1183
Ash 83 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ISO 868
Tensile Strength, Yield 72.0 MPaISO 527-2
Elongation at Yield 35 %ISO 527
Flexural Strength 60.0 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 - 256 °C
Vicat Softening Point 235.6 °CISO 306
Heat Distortion Temperature 220 °CISO 75 A/B
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tisan TISAPET® UNR Polyethylene Terephthalate
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
Akro-Plastic Akromid® B3 LA black (4056) PA6, DAM
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

PTIS072 / 79507

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.