MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shandong Dongyue Shenzhou New Material Co Hexafluoropropene Oxide (HFPO)
Categories: Fluid

Material Notes: Conformable with: Q/DYS 002-2007

Hexafluoropropene Oxide (HFPO) is a kind of colorless and uninflammable gas. It is easy to be liquefied under pressure, and generally be used as special intermediates for fluorine-containing chemicals.

Main Applications:

HFPO is a kind of important intermediates for fluoride material. Being the oxidation product of Hexafluoropropene, it is widely used as intermediates for fluoride compound. It is main component of fluoride vinyl ether product (PPVE/PSVE/PEVE/PMVE), and monomer of fluoride surfactant and PFPE. HFPO can also react through nucleophilic substituent after ring-opening, and it can react as difluoro-carbine under heating.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
@Temperature 25.0 °C
Liquid
Molecular Weight 166 g/mol
Vapor Pressure 6.75 bar
@Temperature 25.0 °C
Saturated
 
Chemical PropertiesOriginal ValueComments
Critical Temperature 86.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point -27.0 °C
 
Descriptive Properties
AppearanceColorless transparent liquid
CAS428-59-1
Chemical NameHexafluoropropene Oxide
Danger Label2.2 (uninflammable, nontoxic gas)
Else (wt%)0.1Excellent
 0.3Grade A
 0.3Qualified
Hexafluoroacetone (HFA) (wt%)0.1Excellent
 0.2Grade A
 0.2Qualified
Hexafluoropropene (HFP) (wt%)0.8Excellent
 4.5Grade A
 9.5Qualified
Hexafluoropropene Oxide (HFPO) (wt%)>90Qualified
 >95Grade A
 >99Excellent
Molecular FormulaC3F6O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSHEN001 / 104056

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.