MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions 140 Series 140X497 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shipping: This resin can be shipped in 45,000 lb bulk trucks and 180,000 lb bulk railcars.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.400 g/ccGeon® 1169
Loss On Ignition 0.10 %Bagged, Geon® 793
Porosity 0.55 %Geon® 1094; DOP Porosity; cc/g
Particle Size 110 µmGeon® 812
Particle Mesh Size 120 Mesh5%; Geon® 812
 230 Mesh5%; Geon® 812
Relative Viscosity 2.32 cP1% Cyclohexanone
Viscosity Measurement 0.97Inherent; ASTM D1243-60-A
 
Descriptive Properties
FormsPowder
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value68No Standard; Correlation
Polymerization ProcessSuspension
Processing MethodElectrostatic Spray Coating
 Fluid Bed Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesElectrical/Electronic Applications
 Fencing & Decking
 Protective Coatings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL0865 / 145434

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.