MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Higlass BJ62A Polypropylene Copolymer, 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: High melt flow, medium high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, high rigidity, excellent processability

Applications: fan blades, fan shrouds

Description: Higlass BJ62A high melt flow, chemically coupled, 30% glass fiber-reinforced polypropylene copolymer has an excellent balance of physically properites and processability.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inTool, Montell
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 66.0 MPa9570 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Modulus 4.10 GPa595 ksiTangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 2.00 J/cm3.75 ft-lb/inASTM D256A
Izod Impact, Unnotched 7.00 J/cm13.1 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FASTM D648
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.60 mm
239 °F
@Thickness 0.0630 in
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene
INEOS Styrolution Absolac 200EP Acrylonitrile Butadiene Styrene (ABS)
Hannam Chemical Hanalac 750 ABS, General Purpose
Edinburg Plastics AGG665 ABS
Edinburg Plastics AGG645 ABS

PMO507 / 53658

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.