MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SAE SiC/AZ91 Magnesium Matrix Composite, as cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Squeeze casting combines gravity die casting with closed die forging in a single operation, resulting in composite products with properties superior to those produced by stir casting, pressureless infiltration, investment casting, or gravity casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 326 MPa47300 psi
Modulus of Elasticity 120 GPa17400 ksi
Poissons Ratio 0.250.25Calculated
Shear Modulus 48.0 GPa6960 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.8 µm/m-°C
@Temperature 20.0 °C
7.67 µin/in-°F
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
Magnesium Elektron Elektron® AZ91 Magnesium Alloy
SAE AZ91 Magnesium Matrix Composite, as cast
Magnesium EA55RS-T4, Extruded
Magnesium EA65RS-T4, Extruded

MMAZ69B / 77769

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.