MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Agility™ 2001 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: Agility 2001 Performance LDPE Resin is a high pressure LDPE resin offering clarity combined with high shrink tension and strength.
Main Characteristics:
  • Optimum LDPE for retail shrink packaging
  • Excellent combination of shrink force and sparkling optics
  • Toughness for demanding applications
. Complies with: US FDA 21 CFR 177.1520 ©2.2. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©2.2

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D792
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 15.4 MPa
@Thickness 0.0508 mm
2240 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Yield, TD 14.1 MPa
@Thickness 0.0508 mm
2050 psi
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, MD 440 %
@Thickness 0.0508 mm
440 %
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, TD 600 %
@Thickness 0.0508 mm
600 %
@Thickness 0.00200 in
ASTM D882
1% Secant Modulus  250 MPa
@Thickness 0.0508 mm
36300 psi
@Thickness 0.00200 in
MD; ASTM D882
 272 MPa
@Thickness 0.0508 mm
39400 psi
@Thickness 0.00200 in
TD; ASTM D882
Elmendorf Tear Strength MD 280 g280 g0.002; ASTM D1922
Elmendorf Tear Strength TD 570 g570 g0.002; ASTM D1922
Dart Drop Test 120 g
@Thickness 0.0508 mm
0.265 lb
@Thickness 0.00200 in
ASTM D1709A
Film Tensile Strength at Break, MD 30.2 MPa
@Thickness 0.0508 mm
4380 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Break, TD 25.4 MPa
@Thickness 0.0508 mm
3680 psi
@Thickness 0.00200 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °F
 
Optical PropertiesMetricEnglishComments
Haze 4.8 %
@Thickness 0.0508 mm
4.8 %
@Thickness 0.00200 in
ASTM D1003
Gloss 91 %
@Thickness 0.0508 mm
91 %
@Thickness 0.00200 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 231 °C448 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance66 ft-lb/in32.0 mil
Film Toughness1140 ft-lb/in3MD, ASTM D882
 1150 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF391 / 311084

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.