MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2740 S-30A Saturated Styrenic Block Copolymer, General Purpose
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 3010 s delay; ASTM D 2240
Tensile Strength at Break 550 psiDie C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tensile Strength, Yield 100 psiASTM D 412
Elongation at Break 700 %Die C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tear Strength 90.0 pliDie C; ASTM D 624
Compression Set 11 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 37 %
@Temperature 158 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 325 - 400 °F
Mold Temperature 60.0 - 100 °F
Drying Temperature 160 °F
@Time 7200 - 14400 sec
Moisture Content 0.040 %
Injection Pressure 5000 - 10000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE)

PQZWA650 / 92131

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.