Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases. Polymerized at low temperatures to give better processing. Provides good tack for rolls and belting |