MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Baydur® PUL 4501 Liquid Polyurethane
Categories: Fluid

Material Notes: Characterization: Baydur PUL 4501 is a two-component liquid polyurethane system for use in composite manufacturing.

Properties / Applications: Baydur PUL 4501 is a two-component liquid polyurethane system for use in composite manufacturing. The isocyanate is a modified diphenylmethane diisocyanate (MDI), and the polyol component is a polyether polyol blend. The system has been specially designed for use in pultrusion and gives excellent composite properties, including superior elongation to failure, shear strength and impact resistance. As with any product, use of the Baydur PUL 4501 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccPolyol (Component B)
 1.24 g/ccIsocyanate (Component A)
 1.80 g/ccM-R-M; ASTM D792
 2.10 g/ccRoving; ASTM D792
Viscosity 60 cPIsocyanate (Component A)
 800 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 7000 psiRoving, transverse; ASTM D683
 11500 psiM-R-M, transverse; ASTM D683
 118000 psiM-R-M, parallel; ASTM D683
 180000 psiRoving, parallel; ASTM D683
Elongation at Break 1.5 %M-R-M
 2.5 %Roving
Flexural Strength 105 MPaRoving, transverse; ASTM D790
 228 MPaM-R-M, transverse; ASTM D790
 758 MPaM-R-M, parallel; ASTM D790
 1460 MPaRoving, parallel; ASTM D790
Shear Strength >= 0.0152 ksiShort beam, Roving, transverse; ASTM D2344
 >= 0.0331 ksiShort beam, M-R-M, transverse; ASTM D2344
 >= 0.0483 ksiShort beam, M-R-M, parallel; ASTM D2344
 >= 0.0627 ksiShort beam, Roving, parallel; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 120 °CRoving
 120 °CM-R-M
 
Processing PropertiesOriginal ValueComments
Gel Time 14.0 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baydur® STR 822 Polyurethane Structural RIM System
Covestro Baydur® 742 IBS Polyurethane Structural Foam RIM, Density 43 pcf
Covestro Baydur® TB 100-15 Polyurethane

PCOVEST0100 / 201883

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.