System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 40% Glass Fiber Filler
Material Notes:
A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.
Information provided by Polyram.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.23
g/cc
ISO 1183
Linear Mold Shrinkage
0.0012
cm/cm
ISO 2577
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
120
MPa
ISO 527
Elongation at Break
2.0 %
ISO 527
Tensile Modulus
10000
MPa
ISO 527
Flexural Strength
200
MPa
ISO 178
Flexural Modulus
6700
MPa
ISO 178
Izod Impact, Notched (ISO)
20.0
kJ/m²
ISO 180
Charpy Impact Unnotched
65.0
kJ/m²
ISO 179
Charpy Impact, Notched
22.0
kJ/m²
ISO 179
Thermal Properties
Original Value
Comments
Melting Point
168
°C
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi)
152
°C
ISO 75
Flammability, UL94
HB
@Thickness 3.00 mm
Flame Spread
22
mm/min
FMVSS302
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Carbon-Core Sphere-mat C IP 250 Chopped strand mat, E-glass Fibers
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Mitsubishi Chemical Advanced Materials Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers (ASTM Product Data Sheet)
DuPont™ Nomex® 450 Aramid Staple Fiber
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers
PPOLYR945 / 126742
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.