MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® A 218 Black 21N Nylon 66, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Product Description: Ultramid® A 218 Black 21N is an unreinforced polyamide 66, standard viscosity, heat stabilized for injection molding. This grade offers all the primary properties of unreinforced polyamide 66. In addition, it has improved resistance to high temperature, and can be used for components which will withstand long-term temperature stresses.

Availability: Africa & Middle East; Asia Pacific; North America

Additive: Heat Stabilizer

Features: Good Mold Release; Heat Stabilized - Inorganic

Use: Consumer Applications; General Purpose; Industrial Applications

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 2.9 %2.9 %Equilibrium, 50% RH; ISO 62
 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527-2
Tensile Strength, Yield 84.8 MPa12300 psiASTM D638
 90.3 MPa13100 psiISO 527-2
Elongation at Break >= 20 %>= 20 %ISO 527-2
Elongation at Yield 4.0 %4.0 %ISO 527-2
 85 %85 %ASTM D638
Tensile Modulus 3.30 GPa479 ksiISO 527-1
Flexural Strength 120 MPa17400 psiISO 178
 125 MPa18100 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiISO 178
 3.30 GPa479 ksiASTM D790
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.99 kJ/m²1.90 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) NBNBISO 180
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.441 J/cm²2.10 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength  22.0 kV/mm
@Thickness 2.00 mm
560 kV/in
@Thickness 0.0787 in
IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
890 kV/in
@Thickness 0.0315 in
IEC 60243-1
Dissipation Factor 0.032
@Frequency 1e+6 Hz
0.032
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 350 V350 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FUnannealed; ISO 75-2/B
 220 °C428 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FUnannealed; ISO 75-2/A
Flammability, UL94  V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
IEC 60695-11-10,-20
 V-2
@Thickness 3.30 mm
V-2
@Thickness 0.130 in
IEC 60695-11-10,-20
Glow Wire Flammability Index 649 °C
@Thickness 1.52 mm
1200 °F
@Thickness 0.0600 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 275 °C509 - 527 °F
Middle Barrel Temperature 270 - 280 °C518 - 536 °F
Front Barrel Temperature 280 - 285 °C536 - 545 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2110 / 310803

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.