MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: TXX145-12"-F155; Various fibers

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 57.0 %Laminate Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4.62 MPa
@Temperature 24.0 °C
Flatwise TS
 1710 MPa
@Temperature 71.0 °C
 1834 MPa
@Temperature 24.0 °C
Tensile Modulus 119 GPa
@Temperature 71.0 °C
 126.2 GPa
@Temperature 24.0 °C
Compressive Yield Strength 1172 MPa
@Temperature 71.0 °C
 1331 MPa
@Temperature 24.0 °C
Compressive Modulus 117 GPa
@Temperature 71.0 °C
Shear Strength 89.6 MPaCompression interlaminar; RT
 71.7 MPa
@Temperature 71.0 °C
Compression interlaminar
 
Descriptive Properties
Cured Thickness per Ply (cm)0.014Laminate
Dry Resin Content (%)38-40Prepreg
Flow (%)4-16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System
Hexcel® HexPly® F155 Epoxy Resin, T2C190 Carbon Tape
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2
Hexcel® HexPly® F155 Epoxy Resin, F3T584 Carbon Fabric

PHEXC102 / 98572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.