MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MarkeTech Aluminum Oxide Ceramic - Alumina 98%  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Data provided by the supplier, MarkeTech International.

Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture, alumina ceramics are the workhorse of engineered ceramics. They are compounded from pure alumina, silica and trace elements to achieve specific properties. Alumina is cast or pressed into sheets, tubes, rods and shapes. For custom engineer ceramics, alumina is often iso-pressed in to large shapes, and while in a chalk like form, can be easily "green machined" to near net shape. After high temperature firing, the parts are then finished machined using diamond tools. Surfaces of alumina can be lapped and polished. The final alumina ceramic can also be metallized, plated and brazed to metal components to form completed parts that are vacuum tight.

MarkeTech International is no longer in business.

Key Words: Al2O3; Aluminium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.97 g/cc
Open Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 210 MPa
Flexural Strength 380 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 9.6
@Frequency 1000 - 1.00e+9 Hz
Dielectric Strength 9.40 kV/mm
@Thickness 2.50 mm
DC @ 0.100 in (2.5 mm) thickness
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.70 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 1650 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 98 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%
Overview - Alumina, 98%, Al2O3
MarkeTech Aluminum Oxide Ceramic - Alumina 97.5%
MarkeTech Aluminum Oxide Ceramic - Alumina 96%
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade

C5MT35 / 356

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.