MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties such as:
  • Transparency
  • Unlimited colorability
  • Stress crack resistance
  • Toughness and stiffness
  • Good chemical resistance
  • EU and FDA food approval
Grilamid TR 55 natural is especially suited for injection molded applications in the application fields of:
  • Optics
  • Automotive
  • Mechanical engineering
  • Safety technology
  • Electro / Electronics
  • Sanitary
  • Domestic appliances
  • Sport & Leisure

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccDry; ISO 1183
Water Absorption 3.5 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 120 MPaConditioned; ISO 2039-1
Tensile Strength, Yield 75.0 MPaDry; ISO 527-1/-2
 75.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 7.0 %Dry; ISO 527-1/-2
 9.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 2200 MPaDry; ISO 527-1/-2
 2200 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 31.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °CLong Term; ISO 2578
 120 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75-1/-2
Glass Transition Temp, Tg 160 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 YesMedical
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsCables & Tubes
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
 Mobile phones and other portable devices
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHeating systems
 Housewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
MedicalUSP VI
OpticsLenses
 Optical components
PackagingCosmetics / Personal care
 Medical packaging
 Non oriented film
ProcessingInjection Molding
 Other Extrusion
Special CharacteristicsTransparent
Water ContactDVGW W270
 KTW
 NSF 61
 WRAS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 55 LX PA12/MACMI
Borosilicate Glass, Low Expansion
Arkema Rilsan® Clear G170 Polyamide
Borosilicate Glass
EMS-Grivory Grilamid® TR 55 LY PA12/MACMI

PGRH096 / 156805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.