ERISYS GE Series glycidyl ether modifiers are low molecular weight epoxy functional products based on alcohols, glycols and phenols. The product line covers a broad range of TSCA approved modifiers from monofunctional to multifunctional materials. Classified at right. Description / Use: 2-Ethylhexyl Glycidyl Ether. Excellent replacement for Butyl Glycidyl Ether as a low viscosity reactive diluent. Information provided by Emerald Performance Materials. |