MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Durethan® BKV 140 000000 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled; Nylon 6, Impact Grade

Material Notes: CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in the dry state

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.6 %1.6 %50% RH; ISO 62
Water Absorption at Saturation 6.0 %6.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0016 cm/cm0.0016 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.0071 cm/cm0.0071 in/in150x105x3; ISO 2577
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 200 MPa29000 psiISO 2093-1
Tensile Strength at Break 180 MPa26100 psi5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 11.5 GPa1670 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 295 MPa42800 psi2 mm/min; ISO 178-A
Flexural Yield Strength 280 MPa
@Strain 3.5 %
40600 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 10.4 GPa1510 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 4.0 %4.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  16.0 kJ/m²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  75.0 kJ/m²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm
@Thickness 1.00 mm
1020 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 V450 VSolution B; IEC 60112
 575 V575 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 213 °C415 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75-1,-2
Vicat Softening Point  >= 200 °C
@Load 5.10 kg
>= 392 °F
@Load 11.2 lb
120°C/h; ISO 306
 >= 200 °C
@Load 5.10 kg
>= 392 °F
@Load 11.2 lb
50°C/h; ISO 306
Oxygen Index 22 %22 %Method A; ISO 4589-2
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
Shrinkage, MD 0.030 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.030 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °F
Mold Temperature 80.0 °C176 °F
Back Pressure 40.0 MPa5800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9544 / 208151

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.