MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
The Chemical Company Adipic Acid, C6H10O4
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Adipic Acid is a mildly toxic, white, crystalline compound. The C6 straight-chain dicarboxylic acid is slightly soluble in water and soluble in alcohol and acetone. Nearly all commercial Adipic Acid is produced from cyclohexane.
Almost 90 percent of Adipic Acid produced is used in the production of nylon 66. The nylon (polyamide) is further processed into fibers for applications in carpeting, automobile tire cord, and clothing. Adipic Acid is also used to manufacture plasticizers and lubricant components.
Food grade Adipic Acid is used as a gelling aid, an acidulant, and as a leavening and buffering agent.
Molecular Formula: C6H10O4

Information provided by The Chemical Company

Key Words: Hexanedioic Acid; CAS Number 124-04-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/cc
Ash <= 0.00050 %
 
Thermal PropertiesOriginal ValueComments
Boiling Point 330 °C
Pour Point 151 °C
Flash Point 196 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %Percent by volume
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe <= 0.000040 %
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Assay= 99.8%
Hazen Color Value (pt-co)= 30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCC001 / 106990

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.