MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK), Very good wear resistance
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Very good wear resistance, dry and lubricated, low melt flow for extrusion and injection molding

AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wear resistance, the resin also offers the outstanding combination of ultra performance attributes commonly known for PEEK. These include: chemical resistance, mechanical strength and stiffness, even at elevated temperatures, as well as long-term and high-temperature thermal-oxidative stability. AV-722 SL30 is formulated with the ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE.) It offers wear resistance performance comparable to PEEK grades with this modifier system while being more cost-effective.

This resin is a low melt flow (high viscosity) grade designed for use in injection molding of less intricate shapes or parts. By virtue of its high viscosity at low shear rates, the resin has high melt strength, and, as such, is extrudable into stock shapes such as rods, pipe, tubing and profile. The resin can be melt processed using conventional equipment and techniques.

Potential applications for AV-722 SL30 include bushings, bearings, wear strips, wear rings, rollers, and other parts or components where sliding friction is encountered. The resin is black in color in its natural state.

Markets/Uses: Automotive / Air Induction / Bushings; Oil & Gas / Down Hole / Bushings and Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Dry

Applications: Automotive Applications; Bearings; Bushings; Oil/Gas Applications; Wear Strip

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; Wear Resistant

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccASTM D792
Water Absorption 0.030 %
@Time 86400 sec
ASTM D570
Viscosity 240 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 1.9 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 82ASTM D785
Tensile Strength 136 MPa5.0 mm/min; ASTM D638
Tensile Strength, Yield 151 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 2.1 %5.0 mm/min; ASTM D638
 2.1 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 12400 MPa5.0 mm/min; ASTM D638
 15700 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 209 MPaISO 178
 213 MPaASTM D790
Flexural Modulus 10200 MPaASTM D790
 13900 MPaISO 178
Compressive Strength 107 MPaASTM D695
Shear Strength 71.0 MPaASTM D732
Izod Impact, Notched 69.0 J/mASTM D256
Izod Impact, Unnotched 450 J/mASTM D256
Izod Impact, Notched (ISO) 7.40 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 30.0 kJ/m²ISO 180
Coefficient of Friction 0.080 - 0.42ASTM D1894
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.34 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.81 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.300 W/m-KASTM C177
Melting Point 340 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 267 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 152 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 354 °C
Middle Barrel Temperature 366 °C
Front Barrel Temperature 371 °C
Nozzle Temperature 374 °C
Melt Temperature 366 - 388 °CInjection
Mold Temperature 149 - 177 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AdditiveCarbon Fiber + Graphite + PTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4156 / 279956

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.