MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AURUM JCF3030 offers a unique balance of mechanical, thermal, and tribological properties for outstanding performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM components offer excellent mechanical strength and toughness, dimensional stability, low outgassing, and exceptional radiation resistance. In addition, AURUM exhibits outstanding resistance to hydraulic, automotive, and many industrial fluids and solvents, a low coefficient of thermal expansion, creep resistance, and flame retardancy. AURUM JCF3030 withstands high PV levels and provides a low wear factor and low friction surface over a broad temperature range in lubricated environments.

Applications: AURUM JCF3030 components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM parts include: thrust washers and oil seal rings for automotive and off road vehicle transmissions, thermal insulators and stripper fingers for high-speed copiers, jet engine components, check valve balls, spline couplings, heat-resistant gears, vanes, wear strips, and valve seats. Other AURUM applications include carriers for aluminum hard disks and silicon wafers, journal bearings, and bearing retainers.

Information provided by DuPont

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
Water Absorption 0.20 %0.20 %24 hrs @ 73°F; ASTM D570
Moisture Absorption at Equilibrium 0.090 %0.090 %73°F; 60 RH, 24hrs
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inASTM D955
Melt Flow  2.0 g/10 min
@Load 2.16 kg,
Temperature 420 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 788 °F
ASTM D1238
 29 g/10 min
@Load 10.0 kg,
Temperature 420 °C
29 g/10 min
@Load 22.0 lb,
Temperature 788 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 170 MPa24600 psiASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 230 MPa33300 psiASTM D790
Flexural Modulus 10.802 GPa1566.7 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 388 °C730 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 246 °C475 °FASTM D648
Glass Transition Temp, Tg 250 °C482 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
Mitsui AURUM® PL450C Polyimide
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade

PMIT045A / 53222

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.