MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hippe PE 300 Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologically safe. Low water absorption, not aromatic-resistant. Manifold usable. Easily machinable. Excellent sliding properties. The abrasion is very low.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 - 0.960 g/ccDIN 53 479
Moisture Absorption at Equilibrium <= 0.050 %Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation <= 0.050 %DIN 53 495
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 54.0 - 60.0 MPa
@Time 30.0 sec
DIN 53 456
Tensile Strength 24.0 - 31.0 MPaDIN 53 455
Elongation at Break 400 - 800 %DIN 53 455
Tensile Modulus 1.00 - 1.40 GPaDIN 53 457
Flexural Modulus 1.00 - 1.40 GPafrom bending test; DIN 53 457
Charpy Impact, Notched NBDIN 53 453
Coefficient of Friction, Dynamic 0.29Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 36in MPa; DIN 53 455
Abrasion 1.0µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmDIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+14 ohmDIN 53 482
Dielectric Constant 2.4
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 150 kV/mmBreakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.00020
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 - 150 µm/m-°C
Specific Heat Capacity 1.70 - 2.00 J/g-°C
Thermal Conductivity 0.350 - 0.430 W/m-K
Melting Point 128 - 133 °CDIN 53 736
Maximum Service Temperature, Air 90.0 °CContinuous use
 120 °CShort Periods
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 85.0 °CISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 42.0 - 49.0 °CISO-R 75 Method A
Glass Transition Temp, Tg -95.0 °Cdynamic; DIN 53 736
Flammability, UL94 HB
 
Descriptive Properties
Colornatural/black
Creep ResistanceGrade KA 3cDIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, sudsresistant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe PE 500 Polyethylene
Chemours 340 PFA Perfluoroalkoxy Copolymer
Overview of materials for Polyester Thermoplastic Elastomer
Celanese Zytel® ST811HS NC010 PA6-HI
CENTROPLAST CENTROFLON Polyvinylidene fluoride

PHIPPE985 / 121989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.