MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Europrene® SOL T 9131 Styrene - Isoprene Block Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Europrene® SOL T 9131 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 15% weight and diblock content is 40%. A non-staining, TNPP free antioxidant system is added during the production process.

Key Features: Europrene® SOL T 9131 is a block copolymer with linear molecular structure and high diblock content, designed for hot melt pressure sensitive applications where improved tackiness and softness, as well as reduced viscosity, are required.

Main Applications: Hot melt pressure-sensitive adhesive for labels or high tack tapes.

Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Brookfield Viscosity 800 cP800 cPToluene sol., 25% wt; ASTM D1084
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 190 °C
10 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Tensile Strength at Break 10.0 MPa1450 psiASTM D412
Elongation at Break 1300 %1300 %ASTM D412
300% Modulus 0.700 MPa
@Strain 300 %
102 psi
@Strain 300 %
ASTM D412

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Europrene® SOL T 9326 Styrene - Isoprene Block Copolymer
Versalis Europrene® SOL T 9113 Styrene - Isoprene Block Copolymer
Versalis Europrene® SOL T 9133 Styrene - Isoprene Block Copolymer
Kraton® D1161 B (SIS) Linear Block Copolymer
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural

PENG215 / 124609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.