MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Superla® 50 White Oil
Categories: Fluid; Lubricant; White Mineral Oil (WMO)

Material Notes: Features

Chevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.

These nearly chemically inert oils are virtually free of nitrogen, sulfur, oxygen and aromatic hydrocarbons. Chevron Superla White Oils contain Vitamin E, a natural antioxidant, to protect quality during handling and storage.

They are clear, bright, and free of solids and water.

Applications

Chevron Superla White Oils find wide application:

  • where direct food contact may occur
  • where prolonged contact with human skin is necessary
  • where odor and staining must be minimized
  • where outstanding long service under adverse conditions is required
Chevron Superla White Oils must be stored in approved containers to prevent contamination that could jeopardize their food grade status.

Key Words: CPS Number: 231067; MSDS Number: 7292
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.870 g/cc
API Gravity 30.4 °
Saybolt Viscosity at 100°F 540 SUS
Kinematic Viscosity at 40°C (104°F) 104 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °CASTM D97
Flash Point 268 °CASTM D92
 
Descriptive Properties
Color+30 minimum, Saybolt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Packers Oil
Chesterton 662 FG Barrier Fluid 22
Anderol ANDEROL® PQ AA 85W140 White Mineral Food Grade Gear Oil, ISO Grade 320, SAE Gear Oil Grade 85W140
Anderol ANDEROL® 40 AA-1 Grease, White Mineral Food Grade NLGI 1
ChevronTexaco Superla® 5 White Oil

WCHEV128 / 74743

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.