MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ML-1130N NAT Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ML-1100 is a general purpose thermoplastic elastomer series, available in NAT and BLK, designed for automotive interior applications. Sarlink ML-1130N NAT is a low hardness, high density, filled grade with good toughness and suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Moldability; Good Tear Strength; Good Toughness; High Density; Low Flow; High Specific Gravity; Low Hardness; Resilient

Uses: Automotive Applications; Automotive Interior Parts; Flexible Grips; General Purpose; Grommets; Knobs; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Viscosity 177 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28
@Time 15.0 sec
Injection Molded; ISO 868
 30
@Time 5.00 sec
Injection Molded; ISO 868
 32
@Time 1.00 sec
Injection Molded; ISO 868
 24.4
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 24.5
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 26.8
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 27.9
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 29.1
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 70.4
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 305 psiFlow, Type 1, 20 in/min; ISO 37
 479 psiAcross Flow, Type 1, 20 in/min; ISO 37
 366 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 397 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 814 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 829 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 79.8 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 146 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 74.0 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 78.4 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 117 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
 123 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
Elongation at Break 470 %Flow, Type 1, 20 in/min; ISO 37
 860 %Across Flow, Type 1, 20 in/min; ISO 37
 517 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 935 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 1060 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 1250 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 70.0 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 93.0 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 15 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 39 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 71 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 94 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Melt Temperature 370 - 410 °F
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1089 / 237580

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.