MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Maxxam™ FR WC-P85 NHFR RoHS Natural Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line speed. It is designed for very thin-wall (0.5 mm or 20 mills), flexible, primary conduit applications for optical fiber cables among others. It is also excellent for injection molding.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4310 sec; ASTM D2240
 48ASTM D2240
Tensile Strength at Break 8.96 MPa51 mm/min; ASTM D638
Elongation at Break 450 %51 mm/min; ASTM D638
Flexural Modulus 296 MPa13 mm/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.55 mm
molded specimen; UL 94
Oxygen Index >= 33 %ASTM D2863
 
Descriptive Properties
FeaturesFlame Retardant
 Good Chemical Resistance
 Good Colorability
 Good Processability
 Halogen Free
 Low Smoke Emission
 Low Toxicity
FormsPellets
Generic MaterialPolyolefin, Unspecified
Generic NamePolyolefin, Unspecified
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityNorth America
RoHS ComplianceRoHS Compliant
UsesConduit
 Corrugated Pipe
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Maxxam™ FR PP 301 Black 1284-11 S Polypropylene
Avient Maxxam™ FR PP 307 Polypropylene
Avient Maxxam™ FR PP 301 S Polypropylene
Avient Maxxam™ FR PP 301 EXT Polypropylene
Avient Maxxam™ FR PE 152 Polyethylene

PH0POL1441 / 146010

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.