MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniLon™ PA6 U GR43 BK1000 Nylon 6, 43% Glass reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: 43% Glass reinforced, utility grade; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Filler Content 43 %ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 171 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 265 MPaASTM D790
Flexural Modulus 12756 MPaASTM D790
Izod Impact, Notched 117 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 480 - 540 °F
Middle Barrel Temperature 500 - 560 °F
Front Barrel Temperature 500 - 560 °F
Nozzle Temperature 520 - 560 °F
Melt Temperature 500 - 560 °F
Mold Temperature 80.0 - 180 °F
Drying Temperature 180 °F
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %
Back Pressure 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Filled
RTP Company RTP 207E TFE 10  Amorphous Nylon (Am. PA) Glass Fiber 40% - PTFE 10%

POMNI5039 / 185185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.