MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC 5338 Mineral Filled, Glass Reinforced Polyester
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in extruded form for ease of handling. Other characteristics are good over all electrical properties and flame resistance.

Typical applications include circuit breaker housings, standoff insulators, bus supports and tool housings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.84 g/cc
Water Absorption 0.10 %24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 35 - 45
Tensile Strength, Ultimate 6000 - 8000 psi
Flexural Strength 19000 - 24000 psi
Compressive Strength 24000 - 28000 psi
Izod Impact, Notched 6.00 - 9.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 350 - 380 V/milShort Time
Arc Resistance >= 190 sec
Comparative Tracking Index >= 600 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 V-0
@Thickness 6.35 mm
 V-0
@Thickness 3.17 mm
 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 5436 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 1412 Flame and Track Resistant

PBMC066 / 27249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.