MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Topcoat™ M Coating Cement
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Fiberfrax Topcoat™ 3000 and Topcoat™ M coating cements have a temperature grade rating of 1538°C (2800°F). Topcoat 3000 consists of a blend of regular ceramic fibers and high-temperature Fibermax® polycrystalline fibers combined with an inorganic binder system. This product imparts excellent flame and hot gas erosion resistance to other product forms and effectively minimizes thermal shrinkage of fiber blankets, modules, and boards. Topcoat M is a blend of Fibermax fibers in a dry powder form which is mixed with a prescribed amount of potable water at the job site. It provides protection against slag and alkali attack when applied to Fiberfrax high-temperature boards and modules.

    Typical Applications
  • Protect high-temperature Fiberfrax lining systems from slag and alkali attack
  • Improve hot gas erosion resistance of Fiberfrax high-temperature linings
  • Reduce thermal shrinkage of hot face in high-temperature refractory and ceramic fiber linings
  • Fill hot face surface cracks

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0411 lb/in³Dry mix
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1454 °C2649 °FRecommended Operating Temperature
Shrinkage 0.30 %
@Temperature 1430 °C,
Time 86400 sec
0.30 %
@Temperature 2610 °F,
Time 24.0 hour
Linear
 
Component Elements PropertiesMetricEnglishComments
Al2O3 73 %73 %
SiO2 21 %21 %
 
Descriptive Properties
AppearanceDry powder
Approx. Coverage 1-Layer (SF/Gal)2.5-5SF/lb (Dry mix)
Temperature Grade (°F)2800
Trace Inorganics (%)3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® TES 40 WN Silicate
Unifrax Fiberfrax® Topcoat™ 3000 Coating Cement

CUNIF041 / 97813

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.