MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Celstran® PPS-CF30-01 PPS, 30% Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Celstran PPS-CF30-01 is a 30% long carbon fiber reinforced polyphenylene sulfide. This material imparts excellent impact and extremlely high modulus properties that exceed that od short carbon fiber PPS.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 203 MPa50mm/min; ISO 527-2/1A
Elongation at Break 0.72 %5mm/min; ISO 527-2/1A
Tensile Modulus 31848 MPa50mm/min; ISO 527-2/1A
Flexural Strength 339 MPaISO 178
Flexural Modulus 30050 MPaISO 178
Charpy Impact, Notched 14.5 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 37.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 29.8 µm/m-°CISO 11359-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
Feed Temperature 20.0 - 50.0 °C
Zone 1 285 - 295 °C
Zone 2 315 - 345 °C
Zone 3 315 - 345 °C
Zone 4 315 - 345 °C
Die Temperature 315 - 345 °C
Melt Temperature 315 - 335 °C
Drying Temperature 110 - 130 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 205 PPS, Unfilled
Celanese Celstran® PPS-GF30-01 PPS, 30% Glass Reinforced
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese FORTRON 203 PPS, Unfilled
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler

PHCQ247 / 178702

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.