MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol VP 3752 Flame retarded epoxy resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Epoxy

Material Notes:

Applications: STRUKTOL VP 3752 is a difunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influenced by introducing phosphorous to the system. Also chemical stabilities are not influenced. These advantages are found when using metal hydroxydes or nonreactive phosphorous substances as flame retardants.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 1.0<= 1.0
 
Electrical PropertiesMetricEnglishComments
High Amp Arc Ignition, HAI 5.2 arcs5.2 arcs
 
Thermal PropertiesMetricEnglishComments
Softening Point 95.0 °C203 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month>= 12.0 Monthin original sealed containers at temperatures less than 40°C
 
Descriptive Properties
AppearanceYellowish resin
Epoxy Equivalent Weight (g/Eq)540

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTRUK66 / 69293

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.