Key Features:- One component, no mix system
- Meets USP Class VI specifications
- Fast setting
- Rapid fixture time
Product Description: Master Bond MB297Med-2 is a single component ethyl cyanoacrylate type adhesive. This high strength, rapid curing system is used primarily for medical device assembly. MB297Med-2 is a lower viscosity (100-110 cps) cyanoacrylate. This kind of system, which is commonly referred to as an instant adhesive or super glue, cures very rapidly with the rate of cure dependent upon the humidity— the higher it is, the faster the cure. Because curing is normally so fast, minimal contact pressure is usually sufficient for bonding. It must be emphasized that this high strength system requires no heating or mixing. It typically sets up within 10-40 seconds depending upon the humidity and the substrates. The bond strength is exceptionally high in the shear mode. MB297Med-2 bonds well to a variety of substrates especially metals, plastics and rubbers. The service temperature range for this system is -60°F to +250°F. Most importantly, MB297Med-2 meets USP Class VI specifications for biocompatibility. MB297Med-2 can be used in a wide array of different medical applications ranging from repair to high speed production. It has first rate resistance to EtO and gamma sterilization processes. Although many of the applications for MB297Med-2 involve disposable type medical devices, it also can be utilized with reusable ones depending upon the service conditions. Product Advantages: - Rapid curing at room temperature; usually sets up within 40 seconds
- No heating or mixing
- Contact pressure usually sufficient for fixturing
- Bonds well to a wide variety of substrates
- Excellent resistance to EtO and gamma sterilization
- Passes USP Class VI testing
- Well suited for disposable and reusable medical devices
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |