MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Essentium High Performance PLA- Annealed Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Essentium PLA has been specifically designed for use in additive manufacturing. Superior tensile strength, modulus and impact resistance in comparison to standard PLA. High heat deflection temperature from excellent heat resistance and faster crystallization rates. Prints with great detail at high speeds, provides less warping, good bed adhesion. Annealed for 110 C for 20 min

Definitions of axes used in property data table: XY is the print direction. ZX is the build direction. YX is the third orthogonal axis.

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccMolded; ISO 1183
Melt Flow 7.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 43.0 MPaZX; ASTM D 638
 55.0 MPaYX; ASTM D 638
 64.0 MPaXY; ASTM D 638
Tensile Modulus 3207 MPaZX; ASTM D 638
 3229 MPaYX; ASTM D 638
 3544 MPaXY; ASTM D 638
Flexural Strength 72.0 MPaZX; ASTM D 638
 92.0 MPaYX; ASTM D 638
 107 MPaXY; ASTM D 638
Flexural Modulus 2874 MPaZX; ASTM D 790
 3266 MPaYX; ASTM D 790
 3414 MPaXY; ASTM D 790
Izod Impact, Notched 60.0 J/mZX; ASTM D 256
 82.0 J/mXY; ASTM D 256
 89.0 J/mYX; ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 - 180 °CASTM D 3418
Maximum Service Temperature, Air >= 100 °CHeat deflection temperature, load unknown; ASTM D 648
Glass Transition Temp, Tg 55.0 - 60.0 °CASTM D 3418
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 240 °CExtrusion Temperature
Nozzle Temperature 235 °C
 
Descriptive Properties
Bed Temperature, °C23-60
Enclosure Temperature, °CRoom Temperature
Print SettingsInfill.: 100%; 30 mm/s, layer height: 0.3mm, extrusion multiplier: 1.0, nozzle diameter: 1.0 mm
Print Speed, mm/s30-70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Essentium High Performance PLA Additive Manufacturing Filament
Overview of materials for Polylactic Acid (PLA) Biopolymer
Clariant Polylactic Acid Natural Color 3D Printer Filament
Clariant Polylactic Acid White 3D Printer Filament
Clariant Polylactic Acid Red 3D Printer Filament

PESSEN906 / 220994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.