MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Petrotene® A3 G10 BRC085 PH405 MSP PP, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: Product Description: 10% Reinforced Glass Fiber, Polypropylene Homopolymer

Resin ID (ISO 1043): PP-GF10
Processing: Injection Molding; Extrusion
Color: White

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792/A
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiASTM D790
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FASTM D648
Vicat Softening Point 120 °C
@Load 5.10 kg
248 °F
@Load 11.2 lb
ASTM D1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL293 / 313201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.