Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machines. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Excellent moisture, oxygen and aroma barriers
- Excellent seal strength and hot tack
- Excellent retention of PVdC seals in humid conditions
- Outstanding optical properties
- Ideal support for water based ink printing on acrylic side
- Water based coatings
Features:- Acrylic Coated
- Flavor & Aroma Barrier
- Gas Barrier
- Humidity Resistant
- In Lamination Lap Sealable
- Moisture Barrier
- Oxygen Barrier
- Very PVdC Coated
Applications:- Bakery
- Biscuits/Cookie/Crackers
- Box Overwrap
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Dairy Products
- Dry Foods and Beverage Powders
- Health and Beauty Care
- Household and Detergents
- Ice Cream
- Pet Food
Uses: - Box Overwrap Flexible Packaging
- HFFS Flexible Packaging
- Pre-made – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |