MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon R3781-920-##R##-P0 Silicone Rubber
Categories: Polymer; Tape; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: This fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tapes become highly crystalline and lose their desirable elastomeric properties. Interleave: 3 mil PE; Rubber: Cured self fusing silicone.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccArlon SQA-TMS-024
Water Absorption 0.40 %MIL-I-46852C
Thickness 20.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D2240
Tensile Strength, Ultimate 1000 psiASTM D412
Elongation at Break 380 %ASTM D412
Adhesive Bond Strength 2.00 psiMIL-I-46852C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 600 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -100 °F
Glass Transition Temp, Tg -117 °CArlon SQA-TMS-055
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 23.9 °C
 
Descriptive Properties
ColorRed
Heat of Crystallization (J/g)4.7DSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Rogers Arlon CP-414R Silicone Rubber
Rogers Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported)
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon R3792-920-10R##-P0 Silicone Rubber

PARL058 / 79710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.